Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 46.2 MPa | 6700 psi | Perpendicular |
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Techmer ES HiFill® PA6 L N MB (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Techmer ES HiFill® PA6 LE BK (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Low Extractables and NucleatedAppearance: BlackTPCI# 7.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Total PSC 524B Polystyrene Polystyrene 524B is a general purpose crystal polystyrene targeted for gloss coextrusion cap applications. It is specially formulated to reduce die buildup and die lines.Information provided by Tota.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Total PSI 940E Impact Polystyrene Description: 940E is a super high impact polystyrene designed for high gloss sheet extrusion and thermoforming applications that require additional toughness.Applications: The combination of high gl.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | 5 lb Core, 6 hrs @ 220°F, Vacuum Bag |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Total PSI 825 Polystyrene Polystyrene 825 is a high impact polystyrene for injection molding. They polymers ability to be molded on fast cycles with minimal stresses results in outstanding impact retention.Applications such .. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
M. Holland Company IS200 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Strength | 46.2 MPa | 6700 psi | ASTM D790 |
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet) |