Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 410 MPa | 59500 psi | |
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec.. |
|||
Flexural Strength | 410 MPa | 59500 psi | |
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Flexural Strength | 410 MPa | 59500 psi | |
GBC Grade 99 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
Flexural Strength | 410 MPa | 59500 psi | |
Sapco S.SiC Silicon Carbide Information provided by Sapco. |
|||
Flexural Strength | 410 MPa | 59500 psi | DIN EN 843-1 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Flexural Strength | 410 MPa @Temperature -40.0 °C |
59500 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Flexural Strength | 410 MPa @Temperature 23.0 °C |
59500 psi @Temperature 73.4 °F |
|
Ceradyne Ceralloy® 546-3E Boron Carbide Features:low porosityhigh puritysingle phaseApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Flexural Strength | 410 MPa @Temperature 23.0 °C |
59500 psi @Temperature 73.4 °F |
|
Ceradyne Ceralloy® 546-4E Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |
|||
Flexural Strength | 410 MPa @Temperature 23.0 °C |
59500 psi @Temperature 73.4 °F |
|
Ceradyne Ceralloy® 546 Boron Carbide Features:neutron absorptionwear resistancehardnesslightweightApplications:semiconductor componentswear componentsballistic armorsputtering targetsnuclear shieldingInformation provided by Ceradyne Co.. |