Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 391 MPa | 56700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu.. |
|||
Flexural Strength | 391 MPa | 56700 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66 LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive. |
|||
Flexural Strength | 391 MPa | 56700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |