Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 379 MPa | 55000 psi | |
Pyrotek TS-207 Thermoset Electrical Insulation Product Polymer reinforcement, Polyester resin, Grey color. High strength and good electrical resistance.Information provided by Pyrotek. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D790 |
PolyOne Edgetek® NN-40CF/000 - OBSOLETE Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D-790 |
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 379 MPa | 55000 psi | |
MTI ThermoStran® PA66-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Strength | 379 MPa | 55000 psi | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Strength | 379 MPa @Strain 3.50 % |
55000 psi @Strain 3.50 % |
ISO 178 |
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface .. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA (Asia Pacific) LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D790 |
Techmer ES HiFill® HDPE TM20 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D790 |
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi.. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM D790 |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 379 MPa | 55000 psi | ASTM F417 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 379 MPa | 55000 psi | MOR; ASTM-F417 |
CoorsTek AD-996 99.6% Alumina |
|||
Flexural Strength | 379 MPa | 55000 psi | MOR; ASTM-F417 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |