Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek TS-207 Thermoset Electrical Insulation Product

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-207 Thermoset Electrical Insulation Product.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polymer reinforcement, Polyester resin, Grey color. High strength and good electrical resistance.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
Water Absorption 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Flexural Strength 379 MPa
55000 psi
Compressive Strength 483 MPa
70100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 215 °C
419 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+8 ohm-cm
3.00e+8 ohm-cm
Dielectric Strength 16.0 kV/mm
406 kV/in
Arc Resistance 183 sec
183 sec