Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Strength | 309 MPa | 44800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10 LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact. |
|||
Flexural Strength | 309 MPa | 44800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66 LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare. |
|||
Flexural Strength | 309 MPa | 44800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV007E PA 66 (Europe-Africa-Middle East) LNP* Verton* RV007E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV007ESS PA 66 (Europe-Africa-Middle East) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific) LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 309 MPa | 44800 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RV007ES PA 66 LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Flexural Strength | 309 MPa | 44800 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific) LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |