Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
Flexural Strength | 24.1 MPa @Temperature 22.8 °C |
3500 psi @Temperature 73.0 °F |
ASTM D790 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Flexural Strength | 24.1 MPa | 3500 psi | |
UCAR Carbon UCAR® SLX Extruded Graphite Densified prior to graphitization, Grade SLX is an extruded graphite with increased densities and strength over SL.Typical Applications:CZ silicon crystal growth Quartz processing Purified electroni.. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Ecomass® 4703ZG92 Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Flexural Strength | 24.1 MPa | 3500 psi | |
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th.. |
|||
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |