Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 228 MPa @Temperature 23.9 °C |
33000 psi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D790 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D 790 |
GEHR Plastics Ultem 2300 PEI-30 GF 30% Glass Fiber Reinforced
(discontinued **) Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and great resistance. It's unique torque strength permits the econom.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR NAT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 HF L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: Lubricated and High FlowAppearance: BlackInformation provi.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66 |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF33 FR HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Flexural Strength | 228 MPa @Temperature 22.8 °C |
33000 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Flexural Strength | 228 MPa | 33000 psi | 10 oz glass cloth laminate |
BCC Products BC 5114 Epoxy Laminating System BC 5114 is a gray low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. For use abov.. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 228 MPa | 33000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |