Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.This grade meets UL94, V-0.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resist.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF33 TL15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Flexural Strength | 224 MPa | 32500 psi | ISO 178 |
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Strength | 224 MPa | 32500 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 224 MPa | 32500 psi | ISO 178 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |