Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco Information provided by PolyOne™ Corporation |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF15 IM1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES HiFill FR® PBT GF30 FR 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 HS L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES HiFill® PEI BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 172 MPa @Temperature 22.8 °C |
25000 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D 790 |
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
(discontinued **) PPO-30 GF is reinforced with 30% glass fiber for higher thermal properties and better dimensional stability. PPO belongs to the group of the amorphous materials and can be used in temperatures rang.. |
|||
Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 GF33 FR HS L BK065 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |