Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 103 MPa @Thickness 3.17 mm, Temperature 22.8 °C |
15000 psi @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D790 |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Techmer ES HiFill® PA4/6 HS LBK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI# 9651150Information provided by TP Composites, Inc. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Techmer ES HiFill® PA6 GF10 TL10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: Heat Stabilizer and PTFE LubricantFeatures: Heat Stabilized and LubricatedInf.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 103 MPa | 15000 psi | Crosswise; ASTM D790 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Flexural Strength | 103 - 124 MPa | 15000 - 18000 psi | |
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c.. |
|||
Flexural Strength | 103 - 131 MPa | 15000 - 19000 psi | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Flexural Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Flexural Strength | 103 - 124 MPa | 15000 - 18000 psi | |
Abatron AboCast 7802-1/AboCure 50-12 Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D570 |
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled
(discontinued **) XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o.. |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet) |
|||
Flexural Strength | 103 MPa | 15000 psi | ASTM D790 |
PolyOne Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |