Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
PolyOne Maxxam™ PPR-20G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
PolyOne Trilliant™ HC HC5210-0020 RS Natural Polypropylene Homopolymer (PP Homopolymer) Information provided by PolyOne |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa @Temperature 130 °C |
13100 psi @Temperature 266 °F |
ASTM D-790 |
Glastic 1120 Corrosion-Resistant Panels Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos.. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di.. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Chase Plastics CP Pryme® AC100-27 Acetal Copolymer Molding Resin Information provided by Chase Plastics. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Chase Plastics CP Pryme® AC100-9 Acetal Copolymer Molding Resin Information provided by Chase Plastics. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 90.3 MPa | 13100 psi | ASTM D790 |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |