Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Plaskolite Optix® CP - 61 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Quantum Polycarbonate Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
I. Stern N1841 General Purpose Crystal Polystyrene Features:Excellent Process PropertiesEasy FlowApplicationsDisplaysToys, CosmeticsAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Ensinger Tecapeek® XP-94 Compression Molded PEEK Compound, 20% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D-790 |
Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ISO 178 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0754 20% Glass, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 89.6 MPa | 13000 psi | ASTM D790 |
Technetics Group Amicon™ Acetal Homopolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |