Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 8.00 MPa | 1160 psi | ASTM D790 |
SABIC MG500026 Linear Low Density Polyethylene for Compounding Product Description: MG500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding applications. It is in the powder form and h.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | (C 203) |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | Y-Direction; IPC-TM-650, 2.4.4 |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | ASTM D790 |
SABIC M500026 Linear Low Density Polyethylene for Injection Molding Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell.. |
|||
Flexural Strength | 8.00 MPa @Temperature 120 °C |
1160 psi @Temperature 248 °F |
ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | Olsen; ASTM D747 |
UBE V210 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | XD; ASTM D790 |
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | XD; ASTM D790 |
DuPont™ Nomex® Type 994, 250 mil Nominal Thickness Rigid Aromatic Nylon Board Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T.. |
|||
Flexural Strength | 8.00 MPa @Temperature 120 °C |
1160 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8255 HS PA6 (Dry) Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and
fle.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | SAE J949 |
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Strength | 8.00 MPa | 1160 psi | ISO 178 |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |