Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 202LV General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products .. |
|||
Flexural Strength | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6460 High Heat Polystyrene Characteristics High impact and modulus Easy flow High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automobile interior pa.. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | ASTM D790 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Flexural Strength | 78.5 MPa | 11400 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-2046HM PCT, 40% Glass Filled Information provided by Samsung Cheil Industries. |