Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 68.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 68.9 MPa
9990 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 68.9 MPa
9990 psi
Crosswise; IPC-TM-650.2.4.4
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced
The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat..
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet)
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow
High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Flexural Strength 68.9 MPa
10000 psi
Northstar Polymers MPP-D80B Rigid Polyurethane
MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus..
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6
Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago.
Flexural Strength 68.9 MPa
10000 psi
initial
Malvern Minerals Nylon with Novacite® L-337 Quartz Filler
Product data demonstrates the effect of the Novacite® (untreated lamellar quartz) filler. A separate entry demonstrates the effect of treated Novakup® filler in nylon. The specific nylon use..
Flexural Strength 68.9 MPa
10000 psi
SGL Carbon Group EK 2241 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES Electrablend® ABS CF10 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo..
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES HiFill® HDPE GF15 50100 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Techmer ES HiFill® HDPE GF20 BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Engineered Polymer Solutions ABS PCR 400, Recycled
General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Flexural Strength 68.9 MPa
10000 psi
Crosswise; ASTM D790
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Flexural Strength 68.9 MPa
10000 psi
ASTM D-790
Axiall 2506 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Flexural Strength 68.9 MPa
10000 psi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® GPA100 ABS
High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved