Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 65.5 MPa | 9500 psi | |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
PolyOne Stat-Tech™ AS-10SS/000 ABS - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790-1 |
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
KYDEX® V103 High Impact Fire-Rated Thermoforming Sheet Features:Formulated to substitute for FR-ABS sheetVery good impact resistanceEasy to form with excellent part definition and deep-draw characteristicsSuggested Applications:Equipment HousingsExhibit.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | |
SGL Carbon Group EK 2209 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® ABS/PBT 1500 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | Type I, 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Techmer ES Electrablend® PA6 IM B Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Conductive, Impact Modified, Heat Stabilized and LubricatedAppearance: Off-WhiteInformation.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D-790 |
Axiall UV-6676 Rigid PVC, Molding Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D-790 |
Axiall 6680 Rigid PVC, Molding, White 476 Georgia Gulf 6680 White 476 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, s.. |
|||
Flexural Strength | 65.5 MPa | 9500 psi | ASTM D790 |
Adell ZS-30 Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |