Mechanical Properties Metric English Comments
Flexural Strength 46.9 MPa
6800 psi
ASTM D790-92
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene
PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase.
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista..
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio..
Flexural Strength 46.9 MPa
6800 psi
at 10 in/min; ASTM D790
M. Holland Company IS410 Polystyrene, High Impact  (discontinued **)
Features: Good Colorability, High Flow, Impact ModifiedUses: Household Goods, Modeling Material, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holl..
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Lucent Polymers TPP-340 Polypropylene, 40% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 46.9 MPa
6800 psi
Max Load; ASTM D790
Spartech PE4130 Reinforced High Density Polyethylene Compound
Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a..
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Ecomass® 1050CO94 Copper Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityCopper Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Technical Polymers
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding
Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing..
Flexural Strength 46.9 MPa
6800 psi
ASTM D-790
Axiall Suprel® 9422 Rigid PVC, Molding
Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with..
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled
Data provided by Adell Plastics, Inc.
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Asahi Kasei Thermofil P-40TC-8100 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Strength 46.9 MPa
6800 psi
0.05 in/min; 3-point; ASTM D790
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap..
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Plaskolite West Optix® CA-1000 IG Clear High Impact Acrylic Resin
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiatio..