Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 414 MPa | 60000 psi | ASTM D-790 |
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Flexural Strength | 414 MPa | 60000 psi | ASTM D790 |
PlastiComp Complet® LCF40-PA66 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Flexural Strength | 414 MPa | 60000 psi | ASTM D790 |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Strength | 414 MPa | 60000 psi | ASTM D790 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 414 MPa | 60000 psi | MOR; ASTM-F417 |
CoorsTek PlasmaPure-UC™ 99.9% Alumina |
|||
Flexural Strength | 414 MPa | 60000 psi | |
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3 Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Flexural Strength | 414 MPa | 60000 psi | IPC TM-650 2.4.4 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Flexural Strength | 414 MPa | 60000 psi | IPC TM-650 2.4.4 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Flexural Strength | 414 MPa | 60000 psi | |
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component.. |
|||
Flexural Strength | 414 MPa | 60000 psi | 20 x 40 mm |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |