Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
PolyOne Maxxam™ PPC-40T Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Quantum PBT Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 41.4 - 58.6 MPa | 6000 - 8500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 435 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | |
SGL Carbon Group EK 204 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES HiFill FR® ABS FR AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and Flame RetardantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES HiFill® HDPE UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | Max Load; ASTM D790 |
Spartech PE4125 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES HiFill® PA6 L UV (Conditioned) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES Luriblend® PE 5902 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES Luriblend® PE 5903 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D 790 |
Styrolution PS 5300 HIPS Excellent ESCRFree of zinc additivesMatte, easily decorated finishGood toughnessUL Classification 94 HBInformation provided by Styrolution |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Total PSI 844E Polystyrene Polystyrene 844E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough ductile sheet with a rich matte finish. 844E is specially formulated to minim.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Ecomass® 4703ZC76 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Asahi Kasei Thermofil P-40CC-1100 40% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
Techmer ES Luriblend® HDPE GL5 Availability: North AmericaForms: PelletsAdditive: Graphite Powder LubricantInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 41.4 MPa | 6000 psi | ASTM D790 |
PolyOne Elastamax® HTE 2101 Thermoplastic Elastomer - PVC/TPU
(discontinued **) Description/Features:InteriorUL 94 V0Applications:General PurposeCustom Profiles-ComplexProcessing Method:Extrusion-Single ScrewInformation provided by PolyOne Corporation. |