Mechanical Properties Metric English Comments
Flexural Strength 391 MPa
56700 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LCF62E PEEK
LNP* THERMOCOMP* LCF62E is a compound based on Polyetheretherketone resin containing 10% Carbon, 30% Glass Fiber fillers. Added features of this material includes: Easy Molding, Electrically Condu..
Flexural Strength 391 MPa
56700 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66
LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive.
Flexural Strength 391 MPa
56700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6
LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers.