Polymer Property : Flexural Strength = 319 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 319 MPa

@Temperature 23.0 °C
46300 psi

@Temperature 73.4 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Flexural Strength 319 MPa
46300 psi
ASTM D-790
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I..
Flexural Strength 319 MPa
46300 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Flexural Strength 319 MPa

@Temperature 23.0 °C
46300 psi

@Temperature 73.4 °F
4; ISO 178
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high ..
Flexural Strength 319 MPa
46300 psi
ISO 178
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
Flexural Strength 319 MPa

@Temperature 23.0 °C
46300 psi

@Temperature 73.4 °F
4; ISO 178
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist..
Flexural Strength 319 MPa
46300 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 319 MPa
46300 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).