Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite West Optix® CA - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
PolyOne Nymax™ 600 A Zip 23 Natural 1 Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Plaskolite West Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Flexural Strength | 121 MPa | 17500 psi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Fiberfil® J-60/40/E8 Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
SABIC Innovative Plastics NORYL S100G20 PPE+PS (Asia Pacific) |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Strength | 121 MPa | 17500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON PE002Z PA 6 LNP* STAT-KON* PE002Z is a compound based on Nylon 6 resin containing 10% Carbon Fiber. Added features of this grade include: Extrusion Grade. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Techmer ES HiFill® ABS GF30 IM 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa @Temperature 22.8 °C |
17600 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECAPET™ PET Polyethylene Terephthalate (PET) TECAPET™ PET is an unreinforced, semicrystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus,.. |
|||
Flexural Strength | 121 - 128 MPa | 17500 - 18500 psi | ASTM D790 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
Flexural Strength | 121 MPa | 17600 psi | ASTM D-790 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |