Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Oxford Polymers C-Acetal 25GF 25% Glass Fiber Reinforced Copolymer Acetal 25% Glass Fiber Reinforced Copolymer AcetalInformation provided by Oxford Polymers. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Oxford Polymers C-Acetal 25GF-BK Acetal, 25% Glass Fiber Reinforced Product Description: Glass Fiber (25% Reinforced), Acetal Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristics: Pre-color.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Ravago Manufacturing Americas Enviramid™ N1300HL BK/UV2 Post Consumer Recycle Nylon 66 Heat Stabilized, Lubricated, UV Stabilized, Black and made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release
(discontinued **) Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft .. |
|||
Flexural Strength | 107 MPa | 15500 psi | |
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/E8 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 107 MPa | 15500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Techmer ES Electrafil® NY-7/EC NAT PA6 |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100HSL (DAM) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Ensinger Hydel® PC-P ESD Polycarbonate (PC) HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM 10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Flexural Strength | 107 MPa | 15500 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Strength | 107 MPa | 15500 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Flexural Strength | 107 MPa | 15500 psi | ASTM D790 |
Fiberfil® J-60/30/E5 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |