Mechanical Properties Metric English Comments
Tensile Stress 45.0 MPa

@Strain 1.00 %,
Temperature 80.0 °C
6530 psi

@Strain 1.00 %,
Temperature 176 °F
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 45.0 MPa

@Strain 1.00 %,
Temperature 80.0 °C
6530 psi

@Strain 1.00 %,
Temperature 176 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 45.0 MPa

@Strain 1.00 %,
Temperature 120 °C
6530 psi

@Strain 1.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 45.0 MPa

@Strain 3.00 %,
Temperature 200 °C
6530 psi

@Strain 3.00 %,
Temperature 392 °F
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of..
Tensile Stress 45.0 MPa

@Strain 2.00 %,
Temperature 200 °C
6530 psi

@Strain 2.00 %,
Temperature 392 °F
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off..
Tensile Stress 45.0 MPa

@Strain 2.00 %,
Temperature 150 °C
6530 psi

@Strain 2.00 %,
Temperature 302 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Tensile Stress 45.0 MPa

@Strain 7.50 %
6530 psi

@Strain 7.50 %
Solvay TECHNYL® A 221 PA66, Conditioned
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Tensile Stress 45.0 MPa

@Strain 0.500 %
6530 psi

@Strain 0.500 %
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi..
Tensile Stress 45.0 MPa

@Strain 6.00 %,
Temperature 80.0 °C
6530 psi

@Strain 6.00 %,
Temperature 176 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 45.0 MPa

@Strain 12.0 %,
Temperature 80.0 °C
6530 psi

@Strain 12.0 %,
Temperature 176 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 45.0 MPa

@Strain 1.00 %,
Temperature 60.0 °C
6530 psi

@Strain 1.00 %,
Temperature 140 °F
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Tensile Stress 45.0 MPa

@Strain 2.00 %,
Temperature 120 °C
6530 psi

@Strain 2.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned
Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co..
Tensile Stress 45.0 MPa

@Strain 40.0 %,
Temperature 80.0 °C
6530 psi

@Strain 40.0 %,
Temperature 176 °F
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 45.0 MPa

@Strain 1.84 %,
Temperature 150 °C
6530 psi

@Strain 1.84 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough..
Tensile Stress 45.0 MPa

@Strain 2.00 %,
Temperature 150 °C
6530 psi

@Strain 2.00 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Stress 45.0 MPa

@Strain 50.0 %,
Temperature 23.0 °C
6530 psi

@Strain 50.0 %,
Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
Tensile Stress 45.0 MPa

@Strain 1.92 %,
Temperature 90.0 °C
6530 psi

@Strain 1.92 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 45.0 MPa

@Temperature 220 °C
6530 psi

@Temperature 428 °F
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Copyright © lookpolymers.com All Rights Reserved