Polymer Property : Tensile Stress = 218 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EH 50A-3S7002 Thermoplastic Elastomer (TPE)
OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t..
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 1.50 MPa

@Strain 300 %
218 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® C4630 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3855 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.50 MPa

@Strain 25.0 %
218 psi

@Strain 25.0 %
Average; ASTM D412 Method A
Seals Eastern 7040 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G44A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G44A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress >= 1.50 MPa

@Strain 100 %
>= 218 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 265A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 1.50 MPa

@Strain 300 %
>= 218 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 565A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 1.50 MPa

@Strain 100 %
>= 218 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 765A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G44A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G44A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 1.50 MPa

@Strain 5.00 %
218 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers