Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.04 MPa @Strain 0.210 %, Temperature 90.0 °C |
1456 psi @Strain 0.210 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Tensile Stress | 10.04 MPa @Strain 0.210 %, Temperature 90.0 °C |
1456 psi @Strain 0.210 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Tensile Stress | 10.04 MPa @Strain 60.5 %, Temperature 100 °C |
1456 psi @Strain 60.5 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 10.04 MPa @Strain 49.19 %, Temperature 120 °C |
1456 psi @Strain 49.19 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |