Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 196 GPa @Temperature 21.0 °C |
28400 ksi @Temperature 69.8 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Modulus of Elasticity | 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Modulus of Elasticity | 196 GPa @Temperature 400 °C |
28400 ksi @Temperature 752 °F |
Dynamic |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |