Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 165 GPa @Temperature 800 °C |
23900 ksi @Temperature 1470 °F |
Dynamic |
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 800 °C |
23900 ksi @Temperature 1470 °F |
Dynamic |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 500 °C |
23900 ksi @Temperature 932 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 600 °C |
23900 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 600 °C |
23900 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 600 °C |
23900 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 600 °C |
23900 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Modulus of Elasticity | 165 GPa @Temperature 649 °C |
23900 ksi @Temperature 1200 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
Modulus of Elasticity | 165 GPa @Temperature 600 °C |
23900 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |