Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Europe-Africa-Middle East) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6018R PC (Asia Pacific) ML6018R is a low viscosity grade exhibiting a high impact performance over standard PC. It contains an enhanced release-agent. Opaque colours only.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.99 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation .. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
8.99 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color .. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -29.0 °C |
8.99 ft-lb/in @Temperature -20.2 °F |
ASTM D256 |
Styron PULSEâ„¢ 2300 PT PC/ABS Engineering Resin Information provided by Styron |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 4500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendGood impact resistance at low temperature, high glossInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm, Temperature -29.0 °C |
8.99 ft-lb/in @Thickness 0.126 in, Temperature -20.2 °F |
0.25 mm Notch Depth, Injection Molded; ASTM D256 |
Styron PULSE™ EXT 100 PC/ABS Engineering Resin Overview: PULSE EXT 100 engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT 100 engin.. |