Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.20 J/cm @Temperature -40.0 °C |
6.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Izod Impact, Notched | 3.20 J/cm @Temperature -40.0 °C |
6.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Izod Impact, Notched | 3.20 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
6.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |