Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Izod Impact, Notched | 0.510 J/cm @Thickness 3.17 mm |
0.955 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.510 J/cm @Thickness 3.17 mm |
0.955 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-5020T SAN, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar EN052 Polyester Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Izod Impact, Notched | 0.510 J/cm @Temperature 23.0 °C |
0.955 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |