Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.430 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0111 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature -40.0 °C |
0.806 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature -30.0 °C |
0.806 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.430 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
0.806 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.430 J/cm @Temperature 23.0 °C |
0.806 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Braskem RP 145 RACO Random Polypropylene Copolymer RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen.. |