Mechanical Properties Metric English Comments
Izod Impact, Notched 0.176 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.330 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibisan® PN107 SAN Resin, General Purpose
Product CharacteristicsWater ClearHigh RigidityMedium FlowInformation provided by Calsak Corporation
Izod Impact, Notched 0.176 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.330 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibisan® PN-117 SAN
Injection Molding
Izod Impact, Notched 0.176 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.330 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibisan® PN-117C SAN
High Clarity
Izod Impact, Notched 0.176 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.330 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Izod Impact, Notched 0.176 J/cm

@Temperature 0.000 °C
0.330 ft-lb/in

@Temperature 32.0 °F
ASTM D256A
Dow 334.03 Developmental Performance Polypropylene Polymer