| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.176 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.330 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Chi Mei Kibisan® PN107 SAN Resin, General Purpose Product CharacteristicsWater ClearHigh RigidityMedium FlowInformation provided by Calsak Corporation |
|||
| Izod Impact, Notched | 0.176 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.330 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Chi Mei Kibisan® PN-117 SAN Injection Molding |
|||
| Izod Impact, Notched | 0.176 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.330 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
| Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
| Izod Impact, Notched | 0.176 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.330 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
| Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
| Izod Impact, Notched | 0.176 J/cm @Temperature 0.000 °C |
0.330 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
| Dow 334.03 Developmental Performance Polypropylene Polymer DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use app.. |
|||