Mechanical Properties Metric English Comments
Izod Impact, Notched 3.00 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
5.62 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid)
Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne
Izod Impact, Notched 3.00 J/cm

@Temperature -30.0 °C
5.62 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
Izod Impact, Notched 3.00 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
5.62 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256
Mapal Plastics Maplon Type H Polypropylene Sheet
Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing..
Izod Impact, Notched 3.00 J/cm

@Thickness 3.17 mm
5.62 ft-lb/in

@Thickness 0.125 in
ASTM Test
Styrolution Terluran® GP-22 ABS
Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and..
Izod Impact, Notched 3.00 J/cm

@Temperature -40.0 °C
5.62 ft-lb/in

@Temperature -40.0 °F
ISO R 180
Styron Pulse® A20-95 PC/ABS
A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 2.5%); ASTM-D256
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Toyobo T-661 Nylon 66, Standard Grade (Conditioned)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Izod Impact, Notched 3.00 J/cm

@Temperature -40.0 °C
5.62 ft-lb/in

@Temperature -40.0 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 3.00 J/cm

@Temperature 0.000 °C
5.62 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene
ABS for sheet and profile extrusionHigh impact resistance, excellent heat resistance, excellent dimensional stability and processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 3.00 J/cm

@Temperature 0.000 °C
5.62 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene
ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 3.00 J/cm

@Temperature 0.000 °C
5.62 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 3.00 J/cm

@Temperature 0.000 °C
5.62 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 3.00 J/cm

@Temperature -20.0 °C
5.62 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene
ABS with high impact resistanceHigh impact resistance at low temperature, high gloss, good processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched >= 3.00 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 5.62 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM Epicarb PC BLACK IQ Polycarbonate
Characteristics: good fluidity, good impact, industrial quality
Izod Impact, Notched 3.00 J/cm

@Temperature 23.0 °C
5.62 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Braskem CP 241 Injection Molding Polypropylene
Description: CP 241 is a high melt flow rate heterophasic copolymer used for general purposes. This product offers excellent processability, easy mould filling, productivity as well as good stiffnes..
Izod Impact, Notched 3.00 J/cm

@Temperature >=23.0 °C
5.62 ft-lb/in

@Temperature >=73.4 °F
ASTM D256
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe
CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade ..