Polymer Property : Impact Test = 42.8 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® FXE173R PC
This data was supplied by SABIC-IP for the Americas region.
Impact Test 58.0 J

@Thickness 3.20 mm
42.8 ft-lb

@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 15 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Impact Test 58.0 J

@Thickness 3.20 mm
42.8 ft-lb

@Thickness 0.126 in
Instrumented Impact, Total Energy; 3.2 mm thick, 15 mph, 3 in. clamp, 0.5 in. dart; ASTM D3763
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Impact Test 58.0 J

@Thickness 3.20 mm
42.8 ft-lb

@Thickness 0.126 in
Instrumented Total Impact; 12.5 mm dart, 75 mm clamp, 3.3 m/s; ASTM D3763
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 58.0 J
42.8 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC
LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added featu..
Impact Test 58.0 J

@Temperature 23.0 °C
42.8 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Asia Pacific)
PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region.