Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 24.0 J | 17.7 ft-lb | multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2382 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2382 engineered polyolefin is designed for large mold-in-color interior applications that require stiffness and dimensional stability. This material exhibits excellent process.. |
|||
Impact Test | 24.0 J | 17.7 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact propertie.. |
|||
Impact Test | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifaxâ„¢ AB220GC/1 Thermoplastic Olefin Resin Key Features: fractional melt flow, high modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, high flexural modulus, high impact strength, good weatherability, good processabilityAppl.. |
|||
Impact Test | 24.0 J @Temperature -30.0 °C |
17.7 ft-lb @Temperature -22.0 °F |
MAII, E at Max Load, Ductile; ISO 6603-2 |
LyondellBasell Hifaxâ„¢ CB229 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processabili.. |
|||
Impact Test | 24.0 J @Temperature 0.000 °C |
17.7 ft-lb @Temperature 32.0 °F |
Multi-Axial Instrumented Impact, Energy at Max Load (Ductile Failure), 6.75 m/sec, 5 lb crosshead; ISO 6603-2 |
LyondellBasell Hostacomâ„¢ CA278A Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA278A is a thermoplastic polyolefin elastomer that is used for automotive interior partsFeatures: Good StiffnessHigh FlowGood MoldabilityGood Impact ResistanceLow Temper.. |
|||
Impact Test | 24.0 J | 17.7 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6 LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 24.0 J | 17.7 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl HS1000X PPE+PS PPE+PS blend. 13% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL 746C f1. Radiant Panel listing. Dielectric strength. Dimensional stability. Suitable for .. |
|||
Impact Test | 24.0 J | 17.7 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |
|||
Impact Test | 24.0 J @Temperature 23.0 °C |
17.7 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon MDM40 PP LNP* Stat-Kon* MDM40 is a compound based on Polypropylene resin containing Mica and Carbon. Characteristics are Statically Conductive.This data was supplied by SABIC-IP for the Americas region. |