Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp DFP22H PC LNP* Lubricomp* DFP22H is a compound based on Polycarbonate containing Glass Fiber and PTFE. Characteristics of this grade are: Internally Lubricated and Healthcare.This data was supplied by SABIC.. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 810HS TPO
(discontinued **) Description: DEXFLEX® 810HS is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. This material is designed to exceed the requirements .. |
|||
Impact Test | 21.0 J @Temperature 5.00 °C |
15.5 ft-lb @Temperature 41.0 °F |
Montell drop weight impact strength |
LyondellBasell Pro-fax SV954 Polypropylene Impact Copolymer Key Features: nucleation shortens cycles for higher productivity, resists dirt and dust pick-up, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling an.. |
|||
Impact Test | 21.0 J @Temperature -30.0 °C |
15.5 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CA199AC Thermoplastic Olefin Resin Key Features: low melt flow, medium low modulus, paintable thermoplastic olefin resin, excellent balance of properties, high toughness, good paintability, flexibleApplications: automotive air bag do.. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific) LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Impact Test | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Impact Test | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Impact Test | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Impact Test | 21.0 J | 15.5 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |