Polymer Property : 300% Modulus = 0.725 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
Polimeri Europa Europrene® SOL TH 2312 Styrene - Ethylene / Butylene Block Copolymer
Europrene® SOL TH 2312 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where b..
300% Modulus 0.00500 GPa
0.725 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00500 GPa
0.725 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Huntsman AVALON® 65 AB Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane
AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh..
300% Modulus 0.00500 GPa
0.725 ksi
0.025" extruded film; DIN 53504
Huntsman IROGRAN® PS455-200 TPU-Polyester
Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 527
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Huntsman AVALON® 65 AK Thermoplastic Polyurethane
Performance Features: AVALON® injection molding products are trusted worldwide to deliver:Outstanding flex performanceExcellent slip resistancePerfect surface definitionTransparency and transluce..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Huntsman AVALON® 70 AE Thermoplastic Polyurethane
Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material ..
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Lubrizol ESTANE® GP70AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 402801S SBS Based Material, 80A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 500750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 502750S SEBS Based Material, Unfilled Qualities, 75A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 502800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 602800S SEBS Based Material, Filled Qualities, 80A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 660750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 662750S SEBS Based Material, Semi-Filled Qualities, 75A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D638
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00500 GPa
0.725 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00500 GPa
0.725 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00500 GPa
0.725 ksi
ASTM D412
Polimeri Europa Europrene® SOL TH 2311 Styrene - Ethylene / Butylene Block Copolymer
Europrene® SOL TH 2311 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where b..
300% Modulus 0.00500 GPa
0.725 ksi
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 62 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..