Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 3000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel lap shear
Resinlab® CYNERGY CA6602 Adhesive
Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel lap shear
Resinlab® CYNERGY CA6702 Adhesive
Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi..
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel lap shear
Resinlab® CYNERGY CA6701 Adhesive
Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal ..
Adhesive Bond Strength 20.7 MPa
3000 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black
Information provided by ITW Devcon
Adhesive Bond Strength 20.7 MPa
3000 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White
Information provided by ITW Devcon
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond F110 Optically Transparent Low Viscosity Epoxy Adhesive
TRA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. This room temperature curing system is an excellent choice for thin bond-line assembly and repair applications of prisms..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Bond F114BK01 Low Viscosity Blush-Free Epoxy Adhesive
TRA-BOND F114BK01 is a low viscosity, room temperature cure, epoxy system that contains no solvents, has excellent wicking and wetting characteristics, and adheres strongly to glass, ceramics, most ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive
TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system..
Adhesive Bond Strength 20.7 MPa
3000 psi
Varies with substrates
Loctite® 312 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum, cured 8 hrs
Tra-Con Tra-Bond 2202 Low Viscosity/High Temperature Epoxy Adhesive
TRA-BOND 2202 is a low viscosity, high temperature cure epoxy resin system developed for rigid laminating, filament winding, potting and bonding applications where a clear, almost transparent adhesi..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive
TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity..
Adhesive Bond Strength 20.7 MPa
3000 psi
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive
Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc..
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel/Steel; Varies with substrates
Loctite® 609 General Purpose Retaining Compound
Retainers: Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies..
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel/Steel; Varies with substrates
Loctite® 640 Medium Strength/High Temperature Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Steel/Steel; Varies with substrates
Loctite® 675 Medium Strength Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Adhesive Bond Strength 20.7 - 41.4 MPa
3000 - 6000 psi
Varies with substrates
Loctite® Durabond® E-214HP Epoxy Adhesive
Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific..
Adhesive Bond Strength >= 20.7 MPa
>= 3000 psi
Lap Shear Strength
Epoxyset Epoxibond EB-106 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
Adhesive Bond Strength >= 20.7 MPa
>= 3000 psi
Lap Shear Strength
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive
A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
Adhesive Bond Strength 20.7 MPa

@Temperature -54.4 °C
3000 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Armstrong C-7/W Epoxy Adhesive, 3:2 Mix Ratio
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 931-1T1N1 Thixotropic Epoxy Encapsulant
TRA-BOND 931-1T1N1 epoxy encapsulant is designed for good adhesion, providing strong resilient bonds to a wide variety of substances. This is a thixotropic version of TRA-BOND 931-1.Information prov..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum, 2 hrs @ 70°C
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive
TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc.
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Bond F114 Optically Clear, Low Viscosity Blush-Free Epoxy Adhesive
TRA-BOND F114 is a clear, low viscosity, room temperature cure, epoxy system with good optical properties that contains no solvents, has excellent wicking and wetting characteristics, and adheres st..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..
Adhesive Bond Strength 20.7 - 34.5 MPa
3000 - 5000 psi
Varies with substrates
Loctite® Durabond® E-20HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Adhesive Bond Strength 20.7 MPa
3000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th..
Adhesive Bond Strength 20.7 MPa
3000 psi
Alum to Alum
Atom Adhesives AA-BOND 2101 Epoxy Adhesive
AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el..
Adhesive Bond Strength 20.7 - 34.5 MPa
3000 - 5000 psi
Varies with substrates
Loctite® Durabond® E-60HP Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Copyright © lookpolymers.com All Rights Reserved