Mechanical Properties Metric English Comments
Modulus of Elasticity 5.00 - 6.00 GPa
725 - 870 ksi
Injection; ISO 527
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Modulus of Elasticity 5.00 - 6.00 GPa
725 - 870 ksi
Injection; ISO 527
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 527
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 527
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 178
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 527
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Injection; ISO 527
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Injection; ISO 527
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Modulus of Elasticity 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 527
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Modulus of Elasticity 2.20 - 6.00 GPa

@Temperature 60.0 - 120 °C
319 - 870 ksi

@Temperature 140 - 248 °F
Average value: 4.02 GPa Grade Count:2
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Modulus of Elasticity 3.80 - 6.00 GPa

@Temperature 60.0 - 120 °C
551 - 870 ksi

@Temperature 140 - 248 °F
Average value: 4.83 GPa Grade Count:2
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Modulus of Elasticity 0.0138 - 6.00 GPa
2.00 - 870 ksi
Average value: 2.34 GPa Grade Count:65
Overview of materials for Epoxy Encapsulant, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o..
Modulus of Elasticity 2.00 - 6.00 GPa
290 - 870 ksi
Average value: 2.67 GPa Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Copyright © lookpolymers.com All Rights Reserved