Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.10 GPa | 450 ksi | ASTM D638 |
Ineos Nova 3504 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Suitable for difficult to fill an thin wall molding, USP Class VIApplications: Cosmetic and medical packaging, Housewares, Consumer Electronic packaging, ToysExposure to gamma r.. |
|||
Modulus of Elasticity | 3.10 - 9.65 GPa | 450 - 1400 ksi | Average value: 6.00 GPa Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Modulus of Elasticity | 3.10 - 9.00 GPa | 450 - 1310 ksi | Average value: 6.38 GPa Grade Count:4 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Modulus of Elasticity | 3.10 - 8.00 GPa | 450 - 1160 ksi | Average value: 5.19 GPa Grade Count:8 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Modulus of Elasticity | 3.10 - 4.14 GPa | 450 - 600 ksi | Average value: 3.54 GPa Grade Count:11 |
Overview of materials for Nylon 612, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | Sample Type 1B, 50 mm/min; ISO 527-1/2:1993 |
Global EPP POM C Acetal Copolymer Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | |
Lehmann & Voss LUVOCOM® 1100-7337/WT Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | DIN 53 504 |
Dow BETAMATE™ 7000/7050 L Epoxy Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | (stiffness), ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 48 Gauge (12 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | (stiffness), ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 65 Gauge (17 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | (stiffness), ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 80 Gauge (20 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | ISO 178 |
Addiplast Addilene J 522 K20 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | GB/T 1040 |
Beijing Evergrow Resources MoS2 Filled Nylon Information provided by Beijing Evergrow Resources. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
BASF Ultramid® A4H PA66 (Dry) Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr.. |
|||
Modulus of Elasticity | 3.10 GPa | 450 ksi | ASTM D638 |
Technetics Group Amicon™ Acetal Homopolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Modulus of Elasticity | 3.10 - 7.00 GPa | 450 - 1020 ksi | Average value: 6.21 GPa Grade Count:12 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Modulus of Elasticity | 3.10 - 37.3 GPa | 450 - 5410 ksi | Average value: 15.1 GPa Grade Count:49 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Modulus of Elasticity | 3.10 - 15.2 GPa | 450 - 2200 ksi | Average value: 5.35 GPa Grade Count:33 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |