Mechanical Properties Metric English Comments
Modulus of Elasticity 0.260 GPa
37.7 ksi
(stiffness), ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Modulus of Elasticity 0.260 GPa
37.7 ksi
(stiffness), ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Modulus of Elasticity 0.260 GPa
37.7 ksi
(stiffness), ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 100 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..
Modulus of Elasticity 0.260 GPa
37.7 ksi
TD; ISO R527-1
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene
LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co.
Modulus of Elasticity 0.260 GPa
37.7 ksi
ASTM D638
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Modulus of Elasticity 0.260 GPa
37.7 ksi
(stiffness), ASTM D882
DuPont™ Clysar® ABL Polyolefin Shrink Packaging Film, 125 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat shrinkable, linear low/ultra low density polyolefin film. Used where lower processing temperatures, superior pack..