Mechanical Properties Metric English Comments
Modulus of Elasticity 1.80 GPa
261 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® ESD 7100
PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject..
Modulus of Elasticity 1.80 GPa
261 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® ESD 7200
PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj..
Modulus of Elasticity 1.80 GPa
261 ksi
4 mm thick;10.0 mm wide molded rod; ISO 178
Premix Thermoplastics PRE-ELEC® PS 1324
PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Modulus of Elasticity 1.80 GPa
261 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Modulus of Elasticity 1.80 - 1.80 GPa

@Temperature 100 - 100 °C
261 - 261 ksi

@Temperature 212 - 212 °F
Average value: 1.80 GPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), High Impact
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a..
Modulus of Elasticity 1.80 - 35.2 GPa
261 - 5100 ksi
Average value: 5.72 GPa Grade Count:175
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Modulus of Elasticity 1.80 - 6.40 GPa
261 - 928 ksi
Average value: 5.16 GPa Grade Count:14
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Modulus of Elasticity 1.80 - 11.0 GPa
261 - 1600 ksi
Average value: 7.95 GPa Grade Count:43
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Modulus of Elasticity 1.80 GPa

@Temperature 20.0 °C
261 ksi

@Temperature 68.0 °F
Micropol Isoplas P651 Crosslinkable Polyethylene
Information provided by Micropol Limited
Modulus of Elasticity 1.80 GPa
261 ksi
ASTM D638
Spartech Royalite R59M Hi-Impact ABS/PVC Resin
Data provided by the manufacturer. A unique ABS/PVC resin that meets the flammability standards of many industries and is a cost-effective alternative to standard fire-rated ABS. High rigidity in t..
Modulus of Elasticity 1.80 GPa
261 ksi
ISO 527-2
Tisan TISLAMID® 66 Impact Modified Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Modulus of Elasticity 1.80 GPa
261 ksi
MD; ExxonMobil Method
ExxonMobil Bicor™ 15MB440 OPP Film
Product Description: Bicor 15MB440 is a biaxially oriented transparent polypropylene film designed to be the outside web of a laminate.Availability: Arica & Middle East, Asia Pacific, Europe, Latin ..
Modulus of Elasticity 1.80 GPa
261 ksi
TD; ExxonMobil Method
ExxonMobil Label-Lyte™ 38DL247 OPP Film
Product Description: A super white opaque, high gloss, high yield and highly cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Av..
Modulus of Elasticity 1.80 GPa
261 ksi
TD; ExxonMobil Method
ExxonMobil Oppalyte™ 38DO447 OPP Film
Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod..
Modulus of Elasticity 1.80 GPa
261 ksi
DIN EN ISO 527
BASF Elastollan R 2001 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Modulus of Elasticity 1.80 GPa
261 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast.
Modulus of Elasticity 1.80 GPa
261 ksi
Conditioned; ISO 178
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead
Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast.
Modulus of Elasticity 1.80 GPa
261 ksi
ASTM D638
Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin
Extrusion Grade Pellets. Excellent blend stock material for impact applications.
Modulus of Elasticity 1.80 - 3.00 GPa
261 - 435 ksi
Average value: 2.34 GPa Grade Count:243
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 1.80 - 3.30 GPa
261 - 479 ksi
Average value: 2.96 GPa Grade Count:19
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 1.80 - 2.41 GPa
261 - 350 ksi
Average value: 2.09 GPa Grade Count:5
Overview of materials for ABS/PVC Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW..