Mechanical Properties Metric English Comments
Modulus of Elasticity 0.900 - 3.50 GPa
131 - 508 ksi
Average value: 1.83 GPa Grade Count:35
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Modulus of Elasticity 0.900 GPa
131 ksi
1 mm/min; ISO 527
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t..
Modulus of Elasticity 0.900 GPa
131 ksi
1 mm/min; ISO 527
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o..
Modulus of Elasticity 0.900 GPa
131 ksi
ISO 527
DSM Fibre Intermediates Nyrim® 1500 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Modulus of Elasticity 0.900 GPa
131 ksi
ISO 527-1/-2
BASF Ultramid® B3L BK00464 PA6 (Conditioned)
Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall ..
Modulus of Elasticity 0.900 - 1.20 GPa
131 - 174 ksi
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Modulus of Elasticity 0.900 GPa
131 ksi
ISO 527
BASF Ultramid® B3L PA6 (Conditioned)
Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing.
Modulus of Elasticity 0.900 GPa
131 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 Nylon 6
Unreinforced, medium viscosityInformation provided by Addiplast.
Modulus of Elasticity 0.900 - 2.65 GPa
131 - 384 ksi
Average value: 1.74 GPa Grade Count:36
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Modulus of Elasticity 0.900 - 2.14 GPa
131 - 310 ksi
Average value: 1.38 GPa Grade Count:15
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler