Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.83 - 33.8 GPa | 700 - 4900 ksi | Average value: 23.6 GPa Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Modulus of Elasticity | 4.83 - 5.52 GPa | 700 - 800 ksi | ASTM D638 |
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo.. |
|||
Modulus of Elasticity | 4.83 GPa | 701 ksi | std. dev. 0.47 GPa |
Schmelzer Industries Pearlveil 110-20 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel.. |
|||
Modulus of Elasticity | 4.83 GPa | 700 ksi | In Tension; ASTM D638 |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
Modulus of Elasticity | >= 4.83 GPa | >= 700 ksi | ASTM D638 |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Modulus of Elasticity | 4.83 GPa | 700 ksi | |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Modulus of Elasticity | >= 4.83 GPa | >= 700 ksi | ASTM D638 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Modulus of Elasticity | 4.83 - 17.2 GPa | 700 - 2500 ksi | Average value: 10.3 GPa Grade Count:28 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |