Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco HARRP™ 20 X 40 Wollastonite HARRP™ 20X40 is suggested for concrete and concrete roof tile reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M325 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco M400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M1250 Wollastonite Fine particle size grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Modulus of Elasticity | 303 GPa | 43900 ksi | Tensile modulus calculated at secant 6000-1000 |
Hexcel® IM8 Carbon Fiber (12,000 Filaments) Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin.. |
|||
Modulus of Elasticity | 303 GPa | 43900 ksi | ASTM C848 |
CoorsTek AD-94 Alumina (nom. 94% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 303 GPa | 43900 ksi | ASTM C848 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Modulus of Elasticity | 303 - 530 GPa @Diameter 0.00300 - 0.150 mm |
43900 - 76900 ksi @Diameter 0.000118 - 0.00591 in |
Fiber Modulus |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |