Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® IM8 Carbon Fiber (12,000 Filaments)

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® IM8 Carbon Fiber (12,000 Filaments).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight/length = 0.446 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin systems. They are used for weaving, braiding, filament winding applications, unidirectional tapes and prepreg tow for fiber placement. Chopped fibers are used in compression and injection molding compounds to produce machine parts, gears, and chemical valves. The finished products have excellent corrosion, creep and fatigue resistance plus high strength and stiffness characteristics.
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5730 MPa
831000 psi
Elongation at Break 1.9 %
1.9 %
Modulus of Elasticity 303 GPa
43900 ksi
Tensile modulus calculated at secant 6000-1000
Copyright © lookpolymers.com All Rights Reserved