| Category | Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer | 
| Manufacturer | Nyco | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Nyco M400 WOLLASTOCOAT® Wollastonite.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Loose | 
| 1.00 g/cc | 0.0361 lb/in³ | Tapped | |
| Density | 2.90 g/cc | 0.105 lb/in³ | |
| Brightness | 87 % | 87 % | G.E. Brightness | 
| Oil Absorption | 23 % | 23 % | |
| Solubility in Water | 0.0095 % | 0.0095 % | |
| Moisture Absorption | 0.100 % | 0.100 % | |
| Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than | 
| 9.5 µm | 9.5 µm | median; Microtrac | |
| <= 30 µm | <= 30 µm | 90% smaller than | |
| pH | 9.9 | 9.9 | 10% Slurry | 
| Specific Surface Area | 1.6 m²/g | 1.6 m²/g | BET | 
| Molecular Weight | 116 g/mol | 116 g/mol | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Mohs | 4.5 | 4.5 | |
| Tensile Strength |           2700 - 4100           MPa           @Diameter 0.00300 - 0.150 mm  | 
                  392000 - 595000           psi           @Diameter 0.000118 - 0.00591 in  | 
        Fiber Strength | 
| Modulus of Elasticity |           303 - 530           GPa           @Diameter 0.00300 - 0.150 mm  | 
                  43900 - 76900           ksi           @Diameter 0.000118 - 0.00591 in  | 
        Fiber Modulus | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
| Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
| Melting Point | 1410 °C | 2570 °F | ASTM D1857 | 
| 1540 °C | 2800 °F | theoretical | 
| Optical Properties | Metric | English | Comments | 
|---|---|---|---|
| Refractive Index | 1.63 | 1.63 | 
| Component Elements Properties | Metric | English | Comments | 
|---|---|---|---|
| Al2O3 | 0.30 % | 0.30 % | |
| CaO | 44.94 % | 44.94 % | |
| Fe2O3 | 0.28 % | 0.28 % | |
| K2O | 0.23 % | 0.23 % | |
| Loss on Ignition(%) | 0.47 % | 0.47 % | |
| MgO | 0.75 % | 0.75 % | |
| MnO | 0.040 % | 0.040 % | |
| SiO2 | 52.94 % | 52.94 % | |
| TiO2 | 0.050 % | 0.050 % | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Electrical Resistivity | 1.30e+13 ohm-cm | 1.30e+13 ohm-cm | pure wollastonite | 
| Dielectric Constant |           6.8                     @Frequency 10000 Hz  | 
                  6.8                     @Frequency 10000 Hz  | 
        |
|           6.8                     @Frequency 100000 Hz  | 
                  6.8                     @Frequency 100000 Hz  | 
        ||
|           6.9                     @Frequency 1.00e+6 Hz  | 
                  6.9                     @Frequency 1.00e+6 Hz  | 
        ||
|           6.9                     @Frequency 1000 Hz  | 
                  6.9                     @Frequency 1000 Hz  | 
        ||
| Dissipation Factor |           0.00152                     @Frequency 1000 Hz  | 
                  0.00152                     @Frequency 1000 Hz  | 
        |
|           0.0046                     @Frequency 10000 Hz  | 
                  0.0046                     @Frequency 10000 Hz  | 
        ||
|           0.0046                     @Frequency 1.00e+6 Hz  | 
                  0.0046                     @Frequency 1.00e+6 Hz  | 
        ||
|           0.0078                     @Frequency 100000 Hz  | 
                  0.0078                     @Frequency 100000 Hz  | 
        
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Appearance | White | |
| Bulking Value (gal./lbs.) | 0.0413 | |
| Minus 400 U.S. Mesh Screen (%) | 99 | |
| Morphology | Acicular |